Product variants
- Primer is a preparatory coating put on materials before painting. Priming ensures better adhesion of paint to the surface, increases paint durability, and provides additional protection for the material being painted. It can also be used to block and seal stains, or to hide a color that is to be painted over.
- Emulsion paint is a water-based paint used for painting interior or exterior surfaces.
- Flat Finish-This finish is generally used on ceilings or walls that are in bad shape. This finish is more forgiving in terms of hiding imperfections in your walls and covers greatly. However this finish provides no washability if you were to get a stain on the wall.
- Matte Finish-This finish is very similar if not the same to the flat finish, but comes with some washability and good coverage.
- Eggshell Finish-This finish has some sheen to it, the equivalence to a shell on an egg. This finish provides great washability, but shows some imperfections on walls. This finish is ideal for bathrooms because it offers not only washability, but has enough shine so water does not stick to it and make it peel.
- Pearl (Satin) Finish-This is very durable in terms of washability and resistance to moisture. It offers the user the full protection on their walls from dirt, moisture, stains, etc. This finish is ideal for bathrooms, furniture, and kitchens, but shows even more imperfections on walls because of its strong shine (this finish is shinier then eggshell).
- Semi-Gloss Finish-This finish is typically used on trim to add detail, elegance, and to show off the wood work. It is used on doors and furniture as well. This is a very high shine, but provides the most protection from moisture and stains on your walls. Obviously this finish shows imperfections on the wall. This finish is generally used in schools and factories where washability and durability are the only considerations.[14]
- Varnish and shellac provide a protective coating without changing the color. They are paints without pigment.
- Wood stain is a type of paint that is very "thin," that is, low in viscosity, and formulated so that the pigment penetrates the surface rather than remaining in a film on the surface. Stain is predominantly pigment or dye and solvent with little binder, designed primarily to add color without providing a surface coating.
- Lacquer is usually a fast-drying solvent-based paint or varnish that produces an especially hard, durable finish.
- An enamel paint is a paint that dries to an especially hard, usually glossy, finish. Enamel paints sometimes contain glass powder or tiny metal flake fragments instead of the color pigments found in standard oil-based paints. Enamel paint is sometimes mixed with varnish or urethane to increase shine as well as assist its hardening process.
- A glaze is an additive used with paint to slow drying time and increase translucency, as in faux painting and Art Painting.
- A roof coating is a fluid applied membrane with elastic properties that allow it to stretch without damage. It provides UV protection to polyurethane foam and is widely used as part of a roof restoration system.
- Fingerpaint is a kind of paint intended to be applied with the fingers; it typically comes in pots and is normally used by children.
- Inks are similar to paints, except they are typically made using finely ground pigments or dyes, and are designed so as not to leave a thick film of binder.
- Anti-graffiti coatings are used to defeat the marking of surfaces by graffiti artists. There are two categories, sacrificial and non-bonding. Sacrificial coatings are clear coatings that allow the removal of graffiti, usually by pressure washing the surface with high-pressure water, removing the graffiti, and the coating (hence, sacrificed). They must be re-applied afterward for continued protection. This is most commonly used on natural-looking masonry surfaces, such as statuary and marble walls, and on rougher surfaces that are difficult to clean. Non-bonding coatings are clear, high-performance coatings, usually catalyzed polyurethanes, that allow the graffiti very little to bond to. After the graffiti is discovered, it can be removed with the use of a solvent wash, without damaging the underlying substrate or protective coating. These work best when used on smoother surfaces, and especially over other painted surfaces, including murals.
- Anti-climb paint is a non-drying paint that appears normal while being extremely slippery. It is usually used on drainpipes and ledges to deter burglars and vandals from climbing them, and is found in many public places. When a person attempts to climb objects coated with the paint, it rubs off onto the climber, as well as making it hard for them to climb.
- Anti-fouling paint, or bottom paint, prevents barnacles and other marine organisms from adhering to the hulls of ships.
- Insulative paint, or insulating paint, reduces the rate of thermal transfer through a surface it's applied to. It consists of any paint with an additive of microspheres that are hollow (vacuum-filled).
- Anti-slip paint contains chemicals to increase the friction of surface so as to prevent them being slippery under-foot, particularly in wet conditions.
Failure of a paint
The main reasons of paint failure after application on surface are the applicator and improper treatment of surface.Application Defects can be attributed to:
- Dilution
- This usually occurs when the dilution of the paint is not done as per manufacturers recommendation. There can be a case of over dilution and under dilution, as well as dilution with the incorrect diluent.
- Contamination
- Foreign contaminants added without the manufacturers consent can cause various film defects.
- Peeling/Blistering
- Most commonly due to improper surface treatment before application and inherent moisture/dampness being present in the substrate.
- Chalking
- Chalking is the progressive powdering of the paint film on the painted surface. The primary reason for the problem is polymer degradation of the paint matrix due to exposure of UV radiation in sunshine and condensation from dew. The degree of chalking varies as epoxies react quickly while acrylics and polyurethanes can remain unchanged for long periods.[15] The degree of chalking can be assessed according to International Standard ISO 4628 Part 6 or 7 or American Society of Testing and Materials(ASTM) Method D4214 (Standard Test Methods for Evaluating the Degree of Chalking of Exterior Paint Films).
- Cracking
- Cracking of paint film is due to the unequal expansion or contraction of paint coats. It usually happens when the coats of the paint are not allowed to cure/dry completely before the next coat is applied. The degree of cracking can be assessed according to International Standard ISO 4628 Part 4 or ASTM Method D661 (Standard Test Method for Evaluating Degree of Cracking of Exterior Paints).
- Erosion
- Erosion is very quick chalking. It occurs due to external agents like air,water etc. It can be evaluated using ASTM Method ASTM D662 (Standard Test Method for Evaluating Degree of Erosion of Exterior Paints).
- Blistering
- Blistering is due to improper surface exposure of paint to strong sunshine. The degree of blistering can be assessed according to ISO 4628 Part 2 or ASTM Method D714 (Standard Test Method for Evaluating Degree of Blistering of Paints).